The application of in situ permeable reactive (zero-valent iron) barrier technology for the remediation of chromate-contaminated groundwater: a field test
摘要:
A small-scale field test was initiated in September 1994 to evaluate the in situ remediation of groundwater contaminated with chromate using a permeable reactive barrier composed of a mixture of zero-valent Fe, sand and aquifer sediment. The site used was an old chrome-plating facility located on a U.S. Coast Guard air base near Elizabeth City, North Carolina. Dissolved chromate concentrations were reduced to less than 0.01 mg/L via reduction from Cr(VI) to Cr(III) as a result of the corrosion of the Fe. As the Fe corrodes, pH increases, oxidation-reduction potential declines, dissolved oxygen is consumed, and Fe(II) is generated. Mineral phases formed as a result of the Fe corrosion include ferrous sulfides and various Fe oxides, hydroxides, and oxyhydroxides.
展开
关键词:
Ranau caldera K-Ar tuff age Sunda subduction oblique convergence slip-partitioning Great Sumatran Fault
DOI:
10.1016/S0883-2927(99)00010-4
被引量:
年份:
1999
相似文献
参考文献
引证文献
辅助模式
引用
文献可以批量引用啦~
欢迎点我试用!